MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Envalior ForTii® K12 PPA-GF40 PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® K12 combines high mechanical strength and good flow ability, ideal for designs requiring dimensional stability and impact resistance. K12 is suitable for applications such as sensor housing or camera bracket. Features: 40% glass reinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³Dry; ISO 1183
Moisture Absorption 1.70 %1.70 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0035 cm/cm0.0035 in/inDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inDry; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psiDry; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %Dry; ISO 527-1/-2
Tensile Modulus 13.5 GPa1960 ksiDry; ISO 527-1/-2
Flexural Strength 330 MPa47900 psiDry; ISO 178
Flexural Modulus 13.5 GPa1960 ksiDry; ISO 178
Charpy Impact Unnotched 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDry; IEC 60093
 >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmCond; IEC 60093
Dielectric Constant  4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
Dry; IEC 60250
 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
Cond; IEC 60250
 5.0
@Frequency 100 Hz
5.0
@Frequency 100 Hz
Dry; IEC 60250
 5.0
@Frequency 100 Hz
5.0
@Frequency 100 Hz
Cond; IEC 60250
Dielectric Strength 33.0 kV/mm838 kV/inDry; IEC 60243-1
 33.0 kV/mm838 kV/inCond; IEC 60243-1
Comparative Tracking Index 600 V600 VDry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FASTM D696
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FASTM D696
Melting Point 325 °C617 °F10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 305 °C581 °FDry; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM7932 / 291368

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.