MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ FR Resin FXD921A Polycarbonate (PC) (Global)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN FXD921A compound is based on Polycarbonate (PC) resin for light diffusion special effects. Color package may affect performance. Added features of this grade include: . Transparent/translucent, Flame Retardant.

Features: Flame Retardant,Translucent,Transparent,Aesthetics & Visual effects

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Water Absorption 0.15 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0200 %Injection Molding
 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62-1
Viscosity 12 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 14.8 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 95.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527
 66.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa50 mm/min; ASTM D638
 63.0 MPa50 mm/min; ISO 527
Elongation at Break 85 %50 mm/min; ISO 527
 125 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa1 mm/min; ISO 527
 2400 MPa50 mm/min; ASTM D638
Flexural Strength 90.0 MPayield, 2 mm/min; ISO 178
 94.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2280 MPa1.3 mm/min, 50 mm span; ASTM D790
 2300 MPa2 mm/min; ISO 178
Izod Impact Notched 760 JASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 73.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 76.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.0
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=3.00 mm
UL 746A
 60 - 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 75.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM E831
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 124 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 123 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 141 °CRate B/50; ISO 306
 142 °CRate B/120; ISO 306
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm
UL 94
 V-0
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 290 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 80.0 - 100 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80490 / 288437

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.