LNP THERMOCOMP KF002L compound is based on POM (Acetal) copolymer resin containing 10% glass fiber. Added features of this grade include: Low Extractables. Features: Low Extractable,High Stiffness,Food Contact Acceptable,Structural Information provided by SABIC |