Product Description: For packaging and food packaging applications- Offers high pinhole resistance, excellent flexibility and abuse resistance
- Excellent sealing characteristics
- Offers toughness, seal properties, optical properties and processability
Complies with: US FDA FCN 424; US FDA-DMF; US USP; EU No 10/2011; Canadian HPFB No Objection (with Limitations). Consult the regulations for complete details. Availability: Asia Pacific; Latin America; North America Additive: Antiblock: No; Processing Aid: No; Slip: No Agency Ratings: DMF; FDA FCN 424; EU No 10/2011; Canadian HPFB No Objection Form: Pellets Processing Method: Blown Film Information provided by The Dow Chemical Company |