MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRICOMP™ DAL22 PC (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
 1.27 g/cc0.0459 lb/in³ISO 1183
Moisture Absorption 0.100 %0.100 %50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow  0.0060 cm/cm
@Time 86400 sec
0.0060 in/in
@Time 24.0 hour
ASTM D955
 0.0060 cm/cm
@Time 86400 sec
0.0060 in/in
@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse  0.0070 cm/cm
@Time 86400 sec
0.0070 in/in
@Time 24.0 hour
ASTM D955
 0.0071 cm/cm
@Time 86400 sec
0.0071 in/in
@Time 24.0 hour
ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psiASTM D638
 57.0 MPa8270 psiISO 527
Tensile Strength, Yield 59.0 MPa8560 psiASTM D638
 59.0 MPa8560 psiISO 527
Elongation at Break 8.0 %8.0 %ISO 527
 8.8 %8.8 %ASTM D638
Elongation at Yield 5.2 %5.2 %ISO 527
 5.3 %5.3 %ASTM D638
Tensile Modulus 2.75 GPa399 ksi50 mm/min; ASTM D638
 2.82 GPa409 ksi1 mm/min; ISO 527
Flexural Strength 84.0 MPa12200 psiISO 178
Flexural Modulus 2.75 GPa399 ksiASTM D790
 3.00 GPa435 ksiISO 178
Izod Impact, Notched 0.580 J/cm1.09 ft-lb/inASTM D256
Izod Impact, Unnotched 7.20 J/cm13.5 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 41.0 kJ/m²19.5 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 J7.38 ft-lbInstrumented Impact Energy @ peak; ASTM D3763
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.280.28ASTM D3702 Modified
Coefficient of Friction, Static 0.180.18ASTM D3702 Modified
K (wear) Factor 42.3 x 10-8 mm³/N-M21.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  69.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 70.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow  55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 55.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
31.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 138 °C280 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 137 °C
@Thickness 3.20 mm
279 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
261 °F
@Thickness 0.126 in
unannealed; ASTM D648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI53539 / 153585

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.