CYCOLOY CX7211 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, medium flow, non chlorinated/brominated flame retardant grade. It has a UL94 V0@1.5mm, 5VA@2.5mm and 5VB@2.0mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications. Features: Hydrolytic Stability,Flame Retardant,Thin Wall,Non-Chlorinated,Non-Brominated,High Flow,Good Mold Release Information provided by SABIC |