Tribocomp® PA66 LGF35 S9 MoS2 is a 35% long glass fiber reinforced high-flow PA66 with a pellet length of 9mm and MoS2. It can easily be processed on most injection molding machines. Applications: Automotive Applications; Automotive Under the Hood; Engineering Parts; Gears; Industrial Applications; Power/Other Tools Features: Abrasion Resistant; Heat Stabilized; High Flow; High Temperature Strength; Low Shrinkage; Medium Friction Injection notes: Pre-drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried. Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 15%, and only regrind of optimum quality should be used. In any case, part properties should be checked. Information provided by Solvay Specialty Polymers. |