MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL™ Resin FE1410PW Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ FE1410PW resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + crystal clear polystyrene (ccPS). This injection moldable material is FC EU, FDA food contact compliant, NSF/ANSI 61*, ACS, WRAS, KTW, and W270 listed for global potable water use. NORYL FE1410PW resin exhibits excellent long-term hydrolytic stability, very low moisture absorption, heat / hot water resistance and is an excellent candidate for a variety of water management applications such as pump housings, impellers, shower/faucet, membrane housings and valves. *NSF certification is color dependent.

Features: Hydrolytic Stability,Low Creep Sensitivity,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Moisture Absorption at Equilibrium 0.060 %0.060 %23°C/50% RH; ASTM D570
Water Absorption at Saturation 0.20 %0.20 %ISO 62-1
Viscosity 32 cP
@Load 10.0 kg,
Temperature 280 °C
32 cP
@Load 22.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 94.0 MPa13600 psi5 mm/min; ASTM D638
 94.0 MPa13600 psi5 mm/min; ISO 527
Elongation at Break 2.7 %2.7 %5 mm/min; ISO 527
 2.8 %2.8 %5 mm/min; ASTM D638
Tensile Modulus 4.77 GPa692 ksi5 mm/min; ASTM D638
 4.93 GPa715 ksi1 mm/min; ISO 527
Flexural Strength 135 MPa19600 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 135 MPa19600 psibreak, 2mm/min; ISO 178
Flexural Modulus 4.86 GPa705 ksi1.3 mm/min, 50 mm span; ASTM D790
 4.88 GPa708 ksi2 mm/min; ISO 178
Izod Impact Notched 35.0 J25.8 ft-lbASTM D256
 35.0 J
@Temperature -30.0 °C
25.8 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 2.30 J/cm4.31 ft-lb/inASTM D4812
 2.25 J/cm
@Temperature -30.0 °C
4.22 ft-lb/in
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 13.0 kJ/m²6.19 ft-lb/in²80*10*4; ISO 180/1U
 13.0 kJ/m²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 1.40 J/cm²6.66 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/2C
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
16.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 126 °C259 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 127 °C
@Thickness 3.20 mm
261 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 140 °C284 °FRate B/120; ISO 306
 146 °C295 °FRate A/50; ISO 306
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 300 °C536 - 572 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 290 - 310 °C554 - 590 °F
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82286 / 290233

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.