MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PoolKemie KEMIEPOX REC 116 + EH212 Epoxy system filled with abrasive fillers
Categories: Polymer; Thermoset; Epoxy

Material Notes: Introduction: Two components epoxy system filled with abrasive fillers. Good mechanical properties. Long pot-life.

Application: Moulds for flexible polyurethane, for rigid polyurethane, simulated wood also of large size on metal frames. Press tools.

Cured: 24 h TA + 15 h 60°C

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 - 1.00 g/cchardener; ASTM D 1475
 1.50 - 1.70 g/ccCured
Water Absorption 0.070 - 0.090 %
@Temperature 25.0 °C,
Time 86400 sec
Cured
 0.40 - 0.50 %
@Temperature 100 °C,
Time 7200 sec
Cured
Viscosity 10 - 12000 cPInitial mixture, EN13702-2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90 - 92Cured; ASTM D 2240
Tensile Strength 24.0 - 28.0 MPaCured; ASTM D 638
Elongation at Break 0.90 - 1.0 %Cured; ASTM D 790
Flexural Strength 40.0 - 45.0 MPaCured; ASTM D790
Flexural Modulus 54000 - 58000 MPaelastic, cured; ASTM D 790
Compressive Strength 68.0 - 72.0 MPaCured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Glass Transition Temp, Tg 70.0 - 75.0 °CCured; ASTM D 3418
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 - 36.0 hourDemoulding time, 15 ml; 6 mm
 10.0 - 15.0 hour
@Temperature 60.0 °C
Post-curing
 
Descriptive Properties
ColorPale yellowHardener
 YellowCured
 YellowResin
Mixing ratio15.5 gweight (for 100 g. RESIN)
 27 mlvolume (for 100 ml. RESIN)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK045 / 318524

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.