Product description: AUROcom® PP HGF40 black compound is a 40% glass fiber reinforced, highly heat stabilized and chemically coupled injection molding grade for automotive exterior applications Typical applications Under the hood housings and ventilators Information provided by Aurora Kunststoffe GmbH |