LNP STAT-KON DE0026E compound is based on Polycarbonate (PC) resin containing 10% carbon fiber. Added features of this grade include: Non-Halogenated Flame Retardant, Electrically Conductive, Easy Molding. Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Non-Chlorinated,Non-Brominated,Electrically Conductive,Easy Molding Information provided by SABIC |