MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BCC Products BC-8360 Urethane Elastomer System
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Applications: BC-8360 is used to make molds of detailed masters that contain shallow undercuts. Some of the most common uses are concrete formliners and to make molds for point-of-purchase displays, rapid prototypes, special effects, taxidermy, and sculpture reproductions.

Characteristics: BC-8360 is a two-part polyurethane molding system. BC-8360 is mixed one-to-one by volume (or 100A-to-95B by weight) and cures at room temperature. BC-8360 contains no fillers and cures to a firm (Shore A60 ± 4), medium amber rubber.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.022 g/ccCurative (Part B)
 1.028 g/ccCured Product
 1.07 g/ccPrepolymer (Part A)
Viscosity 600 cPCurative (Part B)
 2300 cPPrepolymer (Part A)
Storage Temperature 21.0 - 26.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 56 - 64
Tensile Strength, Ultimate 750 psi
Elongation at Break 500 %
Rebound 60 %Bashore
Tear Strength 30.0 plisplit
 150 pliDie C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 minMix Time
 16.0 hourDemold Time
 24.0 hourCure Time
Pot Life 20.0 min
Shelf Life 6.00 MonthPrepolymer (Part A)
 6.00 MonthCurative (Part B)
 6.00 MonthCured Product
 
Descriptive Properties
ColorClearPrepolymer (Part A)
 Light AmberCurative (Part B)
 Medium AmberCured Product
Mix ratio100:96Prepolymer (Part A):Curative (Part B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBCC111 / 250976

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.