MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 1010M Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM 1010M resin is an amorphous, transparent polyetherimide (PEI) plastic offering a glass transition temperature (Tg) of 217C. This inherently flame retardant resin is RoHS compliant. ULTEM 1010M resin is an unreinforced general purpose grade offering high heat resistance, high strength and modulus and broad chemical resistance up to high temperatures with enhanced flow and optimized mold release for metallized reflectors.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.25 %ISO 62-1
Viscosity 13 cP
@Load 5.00 kg,
Temperature 340 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 140 MPaH358/30; ISO 2039-1
Tensile Strength at Break 85.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 105 MPa50 mm/min; ISO 527
Elongation at Break 60 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ISO 527
Tensile Modulus 3300 MPa1 mm/min; ISO 527
Flexural Strength 160 MPayield, 2 mm/min; ISO 178
Flexural Modulus 3300 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Taber Abrasion, mg/1000 Cycles 10CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
Dissipation Factor 0.00050
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0025
@Frequency 2.45e+9 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 VIEC 60112
 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.240 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 195 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 190 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 211 °CRate B/50; ISO 306
 212 °CRate B/120; ISO 306
 215 °CRate A/50; ISO 306
Flammability, UL94 V-0
@Thickness 0.710 mm
UL 94 by SABIC-IP
 5VA
@Thickness 3.00 mm
UL 94 by SABIC-IP
Oxygen Index 44 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 350 - 405 °C
Zone 2 350 - 405 °C
Zone 3 360 - 415 °C
Melt Temperature 370 - 410 °CInjection Molding
Mold Temperature 140 - 180 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Precipitation Temperature 80.0 - 120 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82576 / 290523

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.