MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman CLEARWAY® SF3 De-icer
Categories: Other Engineering Material

Material Notes: Eastman’s de-icers are marketed under the brand name Clearway®. Clearway is acknowledged as one of the leaders in airport runway de-icing and the product range has been developed and expanded to include both liquid and solid formate-based and acetate-based products. Based on sodium formate, Clearway SF3 is an effective solid runway de-icer with low environmental impact. Clearway SF3 melts ice by depressing the freezing point of water and is active at temperatures to -15°C. The irregular-shaped granules will remain where spread. We advise to use the product pre-wetted in combination with corresponding liquid Clearway de-icers to obtain a rapid initial de-icing effect; it can also be applied alone to give a long residual anti-icing effect under extreme weather conditions. The product meets not only all relevant environmental and ecological requirements but also the AMS 1431 standard. Clearway SF3 is classified WGK1*, both for its excellent biodegradability and because of its low aquatic toxicity. Thanks to these properties, this solid de-icing solution carries the Blaue Engel (‘Blue Angel’) ecolabel. When applied with the mechanical facilities of airport maintenance departments, Clearway SF3 allows snow and ice to be removed quickly and economically.

Applications

  • Runway de-icing

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.800 - 0.900 g/cc
Particle Size <= 0.500 µmmax 3%
 >= 2.00 µmmin 90%
 <= 5.00 µmmin 90%
pH 8.00 - 11.0
 
Descriptive Properties
AppearanceWhite, irregular granule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4018 / 323641

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.