MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Forging Brass, UNS C37700, M30 Temper, Shapes
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Hot Extruded

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Hot Formed; Good Suitability – Brazing; Fair Suitability – Butt Weld; Poor Suitability – Capacity for Being Cold Worked

Common Fabrication Processes: Hot Forging and Pressing; hot heading and upsetting; Machining

Typical uses: Decorative Knobs; Door Handles; Furniture Hardware; Valve Bodies for Refrigeration, Chemicals; Golf Putters; Valve Bodies for Agricultural Spray Tanks; Valve Bodies for Scuba & Propane Spray Tanks; Covers; Fuse Bodies; Forgings and Pressings of All Kinds; Valve Components

Applicable Specifications: Bar – Forgings ASTM B124/B124M; Die – Forgings SAE J463, Forgings SAE J461, Forgings AMS 4614; Forgings, Die (Hot Pressed) – ASTM B283/B283M, ASME SB283; Rod – Forgings ASTM B124/B124M, Forgings AMS 4614; Rod, Bar & Shapes – ASTM B981/B981M; Shapes – Forgings ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.305 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 78
@Thickness 25.4 mm
Tensile Strength >= 52.0 ksi
@Thickness 25.4 mm
Tensile Strength, Yield 20.0 ksi
@Thickness 25.4 mm
0.5% Ext
Elongation at Break 45 %
@Thickness 25.4 mm
Tensile Modulus 15000 ksi
Modulus of Rigidity 5600 ksi
Poissons Ratio 0.34Calculated
Machinability 80 %
Forgeability 100 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000640 ohm-cm27% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 69.0 BTU-in/hr-ft²-°F
Melting Point 1620 - 1640 °F
Solidus 1620 °F
Liquidus 1640 °F
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1200 - 1500 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 58 - 61 %
Iron, Fe <= 0.30 %
Lead, Pb 1.5 - 2.5 %
Zinc, Zn 36 - 40.5 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC37700x2 / 292951

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.