MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Go Yen Chemical Goyenchem-AA Anti-Aging Agent for Rubber & Plastic
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Goyenchem-AA overcoming the discoloration of high processing temperature, pollution toward the environment, Goyenchem-AA is eco-friendly within pollution, color changing, which is complete Green product.

Advantages:

  • Goyenchem-AA belongs to innovative Thiourea antiaging agent, which can be applied on rubbery and plastic products, for preventing the cracking and damaging by the ozonidation.
  • Green product with no environmental pollution, discoloration, and no extractive.
  • Unlike traditional anti-aging agent,Goyenchem-AA is suitable for light and colored products.
  • Goyenchem-AA accomplished with heat oxygen accelerated ageingt, aging and fatigue resistant, and oxidant prevention capability.
  • Goyenchem-AA can speed up the curing speed, increase cross linking density, lower down the scorch time and adjust the ulcanization curves while adding into rubbery products.
  • Excellent capacity with rubber and plastic.
  • Participate in the vulcanization process, uneasy migration
  • Perfect capacity of flexing fatigue life
  • Good heat aging preventing
  • Well oxidant prevention
  • Has the influence on curing rate & scorch time
Applications:
  • Different kinds of Natural and synthetic rubbery such as NR, IR, BR, SBR, NBR, CR,CSM and its tapes, plates, molding rubbery products of medical system.
  • Environmental resistant and weather resistant Tires like P tires, heavy industry tires, racing cars tires, and special use tires.
  • Industrial and FMCG rubbery products
  • Textile, printing ink, etc. related industry
  • Related resin, plastic and rubbery industry
  • Polymer and resin who require anti-aging property

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Ash <= 0.20 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 58.0 - 70.0 °C
 
Descriptive Properties
AppearancePowder form
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN370 / 266678

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.