MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-3064 NC Flexible Epoxy Potting Compound & Adhesive
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3064 NC is a filled Epoxy Resin System engineered to give the end user the ability to control the hardness of the cured casting. By varying the mix ratio the hardness can be varied from 60 Shore A to 85 Shore D. 20-3064 NC provides excellent thermal shock resistance and outstanding adhesion. 20-3064 NC LV is a low viscosity version of 20-3064 NC.

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
Viscosity 9800 cPMixed with Catalyst #6 (1:1 Ratio)
 13500 cPMixed with Catalyst #6 (1:1 Ratio)
 17000 cP20-3064RNCLV Epoxy
 29500 cP20-3064RNC Epoxy
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
Hardness, Shore D 80
Tensile Strength 5500 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.3
@Frequency 60 Hz
Dielectric Strength 400 V/mil
Dissipation Factor 0.030
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
Thermal Conductivity 0.430 W/m-K
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
 20.0 min
@Temperature 100 °C
 16.0 - 24.0 hour
@Temperature 25.0 °C
 
Descriptive Properties
ColorBlack
Working Time100 grams mass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX031 / 316708

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.