MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Go Yen Chemical GoyenchemAO-76 Antioxidant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 2082-79-3

GoyenchemAO-76 can be combined with other additives such as costabilizer (e.g. thioesters, phosphites, phosphonites), light stabilizer and other functional stabilizers.

Features:

  • GoyenchemAO-76 can be combined with other additives such as costabilizer (e.g. thioesters, phosphites, phosphonites), light stabilizer and other functional stabilizers. The synergistic blends of GoyenchemAO-76 with GoyenchemAO-168 are extreme performance in polymers stabilization.
Applications:
  • polyolefins: PE, PP

    polymers : styrenics and styrene homo copolymers : IPS, ABS, MBS

  • engineering plastics : PBT, PET and PUR, elastomers like SBS, SBR, BR, adhesives and other organic substrates.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.260 - 0.320 g/cc0.00939 - 0.0116 lb/in³Powder
 0.470 - 0.520 g/cc0.0170 - 0.0188 lb/in³GF
Density 1.02 g/cc0.0368 lb/in³
Volatiles <= 0.50 %<= 0.50 %
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 50.0 - 55.0 °C122 - 131 °F
Flash Point 273 °C523 °F
 
Descriptive Properties
AppearanceWhite, non-flowing powder
Color<25 APHA
 <50 APHA
Solubility<0.01 g/100g solutionWater
 0.6 g/100g solutionMethanol
 1.5 g/100g solutionEthanol
 19 g/100g solutionAcetone
 32 g/100g solutionn-Hexane
 38 g/100g solutionEthylacetate
 40 g/100g solutionCyclohexane
 50 g/100g solutionToluene
 57 g/100g solutionBenzene
 57 g/100g solutionChloroform

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN511 / 266819

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.