MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Konson HEXA-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% Hexamethylene tetramine 20% EPDM/EVA binder and dispersing agents

Use Characteristics: Konson®HEXA-80 is a slightly basic accelerator for slow vulcanization. It causes the cure to start almost as soon as it has been added. The rate of cure as a whole is fairly slow. Konson®HEXA -80 provides a high degree of crosslinking. The compounds containing HEXA-80 receive activation and secondary acceleration from mercapto, sulphenamide, thiuram and dithiocarbamate accelerators. Konson®HEXA-80, in combination with resorcinol, is especially used as a formaldehyde donor for the rubber to metal bonding (steel cords). Rubber to metal bonding is effectively influenced by the excellent dispersion of the granulated chemical. The additional use of an antioxidant is recommended to improve the resistance to ageing of vulcanizates, which have been accelerated by Konson® HEXA-80. Generally blooming does not occur.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective HEXA is assured.

Dosage levels: Accelerator: primary (for thick section articles): 0.6 - 0.8 phr with 3 - 4 phr sulfur;secondary: 0.1 - 0.35 phr with 0.25 - 1.0 phr mercapto or thiuram accelerator and 2.0 - 3.5 phr sulfur Hardening: 10% of total phr of hardening phenolic resin e.g. SP 6700 and SP 6701. For formaldehyde donor: 1.3 - 1.6 phr with 2.5 - 3.2 phr Konson®n R 80;

Applications: Slow-curing compounds, thick section articles, roller coverings, light-colored and transparent articles, formaldehyde donor for resorcinol-based adhesive compounds and hardening phenolic resin-based high hardness compounds.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Mooney Viscosity 35 - 50
@Temperature 50.0 °C
35 - 50
@Temperature 122 °F
Ash <= 0.40 %<= 0.40 %
Evaporation Loss <= 0.30 %<= 0.30 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °F
 
Descriptive Properties
AppearanceWhite or grey-white granules
Content= 98.5 %HEXA
Sieve residue= 0.3 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS009 / 256054

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.