MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Michelman® Michem® 743P Paraffin Emulsion Lube
Categories: Fluid

Material Notes: Michem® Lube 743P exhibits a high degree of water resistance and is used in many water based coating applications to increase water resistance and/or surface slip.

Applications (properties imparted): Can & Coil (lubricity, water resistance), Concrete (water beading, water resistance), Fiber Sizing (slip and lubricity, thermosets compatible
Inks block resistance, mar resistance, rub resistance, water resistance), Nonwovens (block resistance), OEM Applied Wood Protection (water resistance), Overprint Varnishes (water resistance), Thermal Transfer (release).

Handling: Ensure adequate ventilation. Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 - 0.990 g/cc0.970 - 0.990 g/cc
Solids Content 31.5 - 32.5 %31.5 - 32.5 %Non-Volatiles
pH 7.0 - 10.57.0 - 10.5
Brookfield Viscosity <= 150 cP<= 150 cPSpindle #1. 60 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceWhite, low viscosity liquid
Freeze/Thaw StabilityNone: protect from freezing
Recommended pH1.0 - 12.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9844 / 287439

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.