MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem ROBWAX™ 2304 Paraffin wax
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Robwax 2304 is a fully refined paraffin wax derived from petroleum. It has a medium melt point and is filtered for stable color properties. It contains a polymer additive to decrease the stickiness of the granules. Robwax 2304 is used in rubber to give ozone resistance. It is also good for use in candles, paper and paperboard, and a variety of other applications. The high degree of purity makes this wax suitable for many applications, including direct and indirect food use. Robwax 2304 complies with FDA Regulation 21 CFR sections 172.886 Petroleum Wax (direct food additive), and 178.3710 Petroleum Wax (indirect food contact).

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.830 g/cc0.830 g/cc
 
Mechanical PropertiesMetricEnglishComments
Penetration 9.0 - 189.0 - 18Needle
 
Thermal PropertiesMetricEnglishComments
Melting Point 52.2 - 56.7 °C126 - 134 °FASTM D-87
 
Descriptive Properties
AppearanceBead
Color>+28Saybolt
Content<0.5%Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH635 / 315553

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.