Product Description: High Flow Grade. Characteristics: High flow, High impact, Chemical resistant. Availability: Asia Pacific; Europe; North America Features: Chemical Resistant; High Impact Resistance; High Flow Agency Rating: EC 1907/2006 (REACH) UL File Number: E162823Information provided by Formosa Chemicals & Fiber Corporation |