MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR CM6210 PC+ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CM6210 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is a high impact, non chlorinated/brominated mineral filled flame retardant grade that can be injection molded or extruded. It has an MVR (300°C/1.2kg) of 8 and a UL94 V0@1.5mm flame rating.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccASTM D792
Density 1.27 g/ccISO 1183
Water Absorption 0.30 %23°C/sat; ISO 62
Moisture Absorption 0.100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 11.5 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ISO 2039-2
Tensile Strength at Break 50.0 MPa5 mm/min; ASTM D638
 50.0 MPa50 mm/min; ISO 527
 65.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 59.0 MPa5 mm/min; ISO 527
 63.0 MPa50 mm/min; ISO 527
 64.0 MPa5 mm/min; ASTM D638
Elongation at Break 80 %5 mm/min; ASTM D638
 97 %50 mm/min; ISO 527
 101 %5 mm/min; ISO 527
Elongation at Yield 3.5 %50 mm/min; ISO 527
 3.6 %5 mm/min; ISO 527
 4.9 %5 mm/min; ASTM D638
Tensile Modulus 3570 MPa5 mm/min; ASTM D638
 3660 MPa1mm/min; ISO 527
Flexural Yield Strength 106 MPa2 mm/min; ISO 178
 110 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3500 MPa1.3 mm/min, 50 mm span; ASTM D790
 3560 MPa2 mm/min; ISO 178
Izod Impact, Notched 500 J/mASTM D256
 90.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 45.0 kJ/m²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 45.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 45.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 38.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0030
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 52.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
 57.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Thermal Conductivity 0.300 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
 95.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 90.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 106 °CRate B/50; ASTM D1525
 112 °CRate B/50; ISO 306
 114 °CRate B/120; ISO 306
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 1 180 - 225 °CSheet Extrusion
Zone 2 190 - 230 °CSheet Extrusion
Zone 3 205 - 240 °CSheet Extrusion
Zone 4 210 - 245 °CSheet Extrusion
Adapter Temperature 210 - 245 °CSheet Extrusion
Die Temperature 210 - 245 °CSheet Extrusion
Melt Temperature 220 - 245 °C
Roll Temperature 65.0 - 90.0 °CRoll Stack Temp - Bottom
 70.0 - 95.0 °CRoll Stack Temp - Middle
 70.0 - 100 °CRoll Stack Temp - Top
Drying Temperature 80.0 - 90.0 °CSheet Extrusion
Dry Time 3.00 - 4.00 hourSheet Extrusion
 12.0 hourCumulative; Sheet Extrusion
Moisture Content >= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10792 / 244259

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.