SABIC LNP™ THERMOCOMP™ Compound KB006 Acetal (POM) Copolymer
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
Material Notes:
LNP THERMOCOMP KB006 compound is based on POM (Acetal) copolymer resin containing 30% glass bead.
Features: Low Warpage,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.64
g/cc
1.64
g/cc
ASTM D792
Density
1.64
g/cc
0.0592
lb/in³
ISO 1183
Moisture Absorption
0.200 %
0.200 %
23°C/50% RH/24 hrs; ASTM D570
0.200 %
0.200 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.010
-
0.030
cm/cm
0.010
-
0.030
in/in
24hrs; ASTM D955
Linear Mold Shrinkage, Transverse
0.010
-
0.030
cm/cm
0.010
-
0.030
in/in
24hrs; ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
34.0
MPa
4930
psi
5 mm/min; ASTM D638
37.0
MPa
5370
psi
5 mm/min; ISO 527
Elongation at Break
19.8 %
19.8 %
5 mm/min; ASTM D638
20.4 %
20.4 %
5 mm/min; ISO 527
Flexural Strength
43.0
MPa
6240
psi
brk, 1.3 mm/min, 50 mm span; ASTM D790
65.0
MPa
9430
psi
ISO 178
Flexural Modulus
3.99
GPa
579
ksi
1.3 mm/min, 50 mm span; ASTM D790
4.32
GPa
627
ksi
2 mm/min; ISO 178
Izod Impact, Unnotched
3.74
J/cm
7.01
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
4.00
kJ/m²
1.90
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
25.0
kJ/m²
11.9
ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
83.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
46.1
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow
83.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
46.1
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
152
°C
306
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
155
°C
@Thickness 3.20 mm
311
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
107
°C
225
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
103
°C
@Thickness 3.20 mm
217
°F
@Thickness 0.126 in
unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Zone 2
195
-
205
°C
383
-
401
°F
Zone 3
210
-
220
°C
410
-
428
°F
Melt Temperature
200
-
215
°C
392
-
419
°F
Injection Molding
Mold Temperature
80.0
-
110
°C
176
-
230
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81646 / 289593
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.