MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cabot CABELEC® XS6324B PE, Conductive Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product highlights: CABELEC XS6324B conductive concentrate is an electrically conductive concentrate made from a well-selected carbon black finely dispersed in polyethylene resins. Its electrical and mechanical properties are not dependent on atmospheric conditions however, they depend on the type and level of dilution of the resin used and the processing conditions. Unlike standard conductive compounds, which have very limited dilution potential, CABELEC XS6324B conductive concentrate has the potential to be diluted with a high quantity of natural resin. This allows users of CABELEC XS6324B conductive concentrate to benefit from the versatility of this concentrate and from the enhanced physical properties due to higher levels of dilution resin.

Key applications: CABELEC XS6324B conductive concentrate can reduce the hazards of electrostatic discharge in applications such as polypropylene based conductive slit tape, polypropylene Flexible Intermediate Bulk Containers (FIBCs), monofilament and other extrusion and molding applications.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Melt Flow 6.0 g/10 min
@Load 190 kg,
Temperature 21.6 °C
6.0 g/10 min
@Load 419 lb,
Temperature 70.9 °F
ISO 1133
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 230 °C392 - 446 °FExtrusion
Drying Temperature 90.0 °C194 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT063 / 315798

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.