MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin AUT195M Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method). Contains low level of mold release.

Features: High Heat Resistance,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.26 g/ccASTM D792
Density 1.26 g/ccISO 1183
Moisture Absorption 0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.90 %ISO 62-1
Viscosity 16 cP
@Load 5.00 kg,
Temperature 340 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 24 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPa50 mm/min; ISO 527
 85.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 95.0 MPa50 mm/min; ISO 527
 97.0 MPa5 mm/min; ASTM D638
Elongation at Break 20 %50 mm/min; ISO 527
 70 %5 mm/min; ASTM D638
Elongation at Yield 6.5 %50 mm/min; ISO 527
 7.0 %5 mm/min; ASTM D638
Tensile Modulus 3000 MPa1 mm/min; ISO 527
 3300 MPa5 mm/min; ASTM D638
Flexural Strength 125 MPayield, 2 mm/min; ISO 178
 145 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3100 MPa2 mm/min; ISO 178
 3170 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 53.0 JASTM D256
 55.0 J
@Temperature -30.0 °C
ASTM D256
 2670 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 2083 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 4.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.230 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 195 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 180 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 187 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 191 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 200 °CRate B/50; ISO 306
 205 °CRate B/120; ISO 306
 209 °CRate B/50; ASTM D1525
 210 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 340 - 360 °C
Zone 2 330 - 350 °C
Zone 3 340 - 360 °C
Melt Temperature 340 - 380 °CInjection Molding
Mold Temperature 125 - 140 °C
Drying Temperature 130 - 140 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Precipitation Temperature 80.0 - 100 °CHopper Temperature
 
Descriptive Properties
Metallized Haze Onset195 °CSABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82663 / 290610

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.