MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC GELOY™ XP4025 ASA (Americas)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA. Excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Water Absorption 0.24 %24 hours; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.7 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 18 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 31 g/10 min
@Load 3.80 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114ASTM D785
Tensile Strength at Break 45.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 58.0 MPa50 mm/min; ISO 527
 59.0 MPa50 mm/min; ASTM D638
Elongation at Break 25 %50 mm/min; ASTM D638
 64 %50 mm/min; ISO 527
Elongation at Yield 4.1 %50 mm/min; ISO 527
Tensile Modulus 2400 MPa1mm/min; ISO 527
Flexural Yield Strength 80.0 MPa2 mm/min; ISO 178
 88.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2400 MPa2 mm/min; ISO 178
 2580 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 170 J/mASTM D256
 64.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 21.0 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 37.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 39.0 JASTM D3763
 33.0 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
Thermal Conductivity 0.250 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 107 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 102 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 109 °CRate B/50; ISO 306
UL RTI, Electrical 50.0 °CUL 746B
UL RTI, Mechanical with Impact 50.0 °CUL 746B
UL RTI, Mechanical without Impact 50.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.47 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Gloss 90 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 255 °CInjection Molding
Zone 1 220 - 230 °CSheet Extrusion
 230 - 250 °C
Zone 2 230 - 245 °CSheet Extrusion
 240 - 255 °C
Zone 3 245 - 255 °CSheet Extrusion
 245 - 260 °C
Zone 4 255 - 265 °CSheet Extrusion
Adapter Temperature 255 - 265 °CSheet Extrusion
Die Temperature 255 - 265 °CSheet Extrusion
Melt Temperature 255 - 270 °C
 255 - 270 °C
Mold Temperature 55.0 - 70.0 °C
Roll Temperature 75.0 - 90.0 °CRoll Stack Temp - Bottom
 95.0 - 110 °CRoll Stack Temp - Middle
 100 - 120 °CRoll Stack Temp - Top
Drying Temperature 90.0 - 100 °CInjection Molding
 90.0 - 100 °CSheet Extrusion
Dry Time 3.00 - 4.00 hourInjection Molding
 3.00 - 4.00 hourSheet Extrusion
 8.00 hourCumulative; Injection Molding
 8.00 hourCumulative; Sheet Extrusion
Moisture Content >= 0.040 %
 0.040 %
Back Pressure 0.300 - 1.00 MPa
Shot Size 40 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10147 / 243614

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.