LNP COLORCOMP D10008FR compound is based on Polycarbonate (PC) resin. Added features of this grade include: Flame Retardant, Mold Release, Superior Molding. Features: Aesthetics and Appearance,Superior Molding,Custom Color,Flame Retardant,Good Mold Release Information provided by SABIC |