Product Description: HD3300-GP is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. HD3300-GP is characterized by a high melt index which allows easy processing of medium to thing-walled articles. Its uses include injection molding for containers Availability: Africa & Middle East; Asia Pacific; Europe; Latin America Features: Copolymer; Good Impact Resistance; Good Processability; Good Rigidity; High Density; High Gloss; Narrow Molecular Weight Distribution Uses: Containers Processing Method: Injection Molding Information provided by Osterman & Company |