LNP LUBRICOMP JCL36 compound is based on Polyethersulfone (PES) resin containing 30% carbon fiber, 15% PTFE. Added features of this grade include: Internally Lubricated, Wear Resistant, Electrically Conductive. Features: Internally Lubricated,Light-weight Structural,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive,Structural Information provided by SABIC |