MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LEXAN™ Copolymer SLX2432T Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.

Features: Weatherable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Water Absorption 0.12 %
@Time 86400 sec
0.12 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.170 %0.170 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %0.25 %ISO 62-1
Viscosity 9.0 cP
@Load 1.20 kg,
Temperature 300 °C
9.0 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 69.0 MPa10000 psi50 mm/min; ISO 527
 72.0 MPa10400 psi50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ISO 527
 67.0 MPa9720 psi50 mm/min; ASTM D638
Elongation at Break 110 %110 %50 mm/min; ASTM D638
 110 %110 %50 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 2.55 GPa370 ksi50 mm/min; ASTM D638
 2.55 GPa370 ksi1 mm/min; ISO 527
Flexural Strength 105 MPa15200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 105 MPa15200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.50 GPa363 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.50 GPa363 ksi2 mm/min; ISO 178
Izod Impact Notched 700 J516 ft-lbASTM D256
 98.0 J
@Temperature -30.0 °C
72.3 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 26.0 J/cm48.7 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 25.0 kJ/m²11.9 ft-lb/in²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 3.00 J/cm²14.3 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 77.0 J56.8 ft-lbASTM D3763
 85.0 J
@Temperature -40.0 °C
62.7 ft-lb
@Temperature -40.0 °F
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=1.50 mm
0.00 - 15 arcs
@Thickness >=0.0591 in
UL 746A
 15 - 30 arcs
@Thickness >=3.00 mm
15 - 30 arcs
@Thickness >=0.118 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 130 °C
@Thickness 3.20 mm
266 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 116 °C241 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 118 °C
@Thickness 3.20 mm
244 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 135 °C275 °FRate B/50; ASTM D1525
 135 °C275 °FRate B/50; ISO 306
 137 °C279 °FRate B/120; ISO 306
UL RTI, Electrical 110 °C230 °FUL 746B
UL RTI, Mechanical with Impact 110 °C230 °FUL 746B
UL RTI, Mechanical without Impact 110 °C230 °FUL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm
V-2
@Thickness >=0.0591 in
UL 94
Oxygen Index 38 %38 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.591.59ASTM D542
Haze 0.80 %
@Thickness 2.54 mm
0.80 %
@Thickness 0.100 in
ASTM D1003
Transmission, Visible 84 %
@Thickness 2.54 mm
84 %
@Thickness 0.100 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 275 - 295 °C527 - 563 °F
Zone 2 265 - 290 °C509 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80422 / 288369

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.