MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Materion QR12 Capacitor Grade Tantalum
Categories: Metal; Nonferrous Metal; Refractory Metal; Pure Element

Material Notes: Minimum standards for Capacitor Grade Tantalum Powders

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 62.0 - 70.0 g/ccScott
Particle Mesh Size -325 Mesh<55%
 40.0 Mesh0 percent
 
Processing PropertiesOriginal ValueComments
Sintering Temperature 1800 °CElectrical Test 1
 2050 °CElectrical Test 2
 
Component Elements PropertiesOriginal ValueComments
Calcium, Ca <= 0.000200 %<2 ppm
Carbon, C <= 0.00300 %<30 ppm
Chromium, Cr <= 0.00100 %<10 ppm
Copper, Cu <= 0.000200 %<2 ppm
Iron, Fe <= 0.00250 %<25 ppm
Molybdenum, Mo <= 0.000500 %<5 ppm
Nickel, Ni <= 0.00100 %<10 ppm
Niobium, Nb (Columbium, Cb) <= 0.00100 %<10 ppm
Nitrogen, N <= 0.00400 %<40 ppm
Oxygen, O <= 0.110 %<1100 ppm
Potassium, K <= 0.00100 %<10 ppm
 
Descriptive Properties
Crush>12 lb7.5 dg)
Fisher Subsieve Sizer FAPD11.5-14.5 Micron

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NBB92173 / 323531

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.