MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TSRC Taipol® 1778 Styrene Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Polymerization System: Cold polymerized emulsion

Emulsifier: Mixed Acid Soap

Stabilizer: Non-Staining, non-discoloring

Coagulant: Acid

Extender: Semi-paraffinic oil, 37.5 parts

Characteristics: Light colored and excellent processing properties.

Application: Hoses, sports goods, shoe soles, conveyor belt, tire and other industrial products.

Test Recipe, ASTM D-3185
Taipol SBR-1778 – 137.5
Zinc oxide - 3.00
Stearic acid - 1.00
Sulfur - 1.75
HAF black(IRB#9) – 68.75
TBBS - 1.38
Total – 213.38

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.75 %ASTM D-5668
Mooney Viscosity 40 - 54
@Temperature 100 °C
ML1+4; ASTM D-1646
Ash <= 1.0 %ASTM D-5667
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22.5 - 24.5 %Bound; ASTM D-5775
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 160 kg(f)/cm²Cure @ 35 min for 145?; ASTM D-412
Elongation at Break >= 380 %Cure @ 35 min for 145?; ASTM D-412
300% Modulus 65.0 - 105 kg(f)/cm²Cure @ 25 min for 145?; ASTM D-412
 90.0 - 130 kg(f)/cm²Cure @ 35 min for 145?; ASTM D-412
 110 - 150 kg(f)/cm²Cure @ 50 min for 145?; ASTM D-412
 
Descriptive Properties
Organic Acid3.9-5.7%ASTM D-5774
Soap<0.5%ASTM D5774

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTSRC008 / 306296

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.