Description: Styrene-butadiene rubber SKS-30 ARKM-27 (SBR-1712) is a styrene and butadiene copolymer obtained by emulsification method with the use of mixture of rosin and fatty acids soaps. The rubber is filled with extender DAE-type oil for synthetic rubbers. REACH: registered Application: widely used in industrial rubber industries. Appearance: briquettes (bales) Color: from light-brown to dark-brown Information provided by JSC, Synthez-Kauchuk |