MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Markforged Smooth TPU 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Smooth TPU (Thermoplastic Polyurethane) is an elastomeric material ideal for functional parts requiring elongation and flexibility. You can print drive belts, bumpers, protective coverings, gaskets, and more with a smooth surface finish and high reliability. Markforged S-TPU is available in black and white colors.

Applications:

  • Seals and gaskets
  • Shock absorbers
  • Protective coverings
  • Straps, bands, and drive belts
  • Non-marring work holding and grips
  • Wheels and treads

Information provided by Markforged, Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/inĀ³D792-20 (Method A)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595D2240-15 (Type A)
Tensile Strength at Break 26.0 MPa3770 psiD412-16
Elongation at Break 550 %550 %D412-16
Tensile Modulus  0.0130 GPa
@Strain 100 %
1.89 ksi
@Strain 100 %
D412-16
 0.0980 GPa
@Strain 2 %
14.2 ksi
@Strain 2 %
D412-16
Flexural Strength 130 MPa18900 psiFlex Elongation at Break = 4%; ASTM D790
Flexural Modulus 0.0900 GPa13.1 ksiASTM D790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARKF997 / 322755

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.