MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sipchem EVA 0818 LO 18% Ethylene Vinyl Acetate copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Product description: Sipchem EVA 0818 LO is a 18% ethylene vinyl acetate copolymer resin, designed for film applications. EVA 0818 LO exhibits high transparency, good mechanical properties and low gel level. It is manufactured by IPC, an affiliate of Sipchem in The Kingdom of Saudi Arabia using an Exxon Mobil high-pressure tubular process.

Applications: Blend Partner, Stretch Film, Stretch Hood, Co-Extrusion Film.

Additives: Thermal Stabilizer: 500 ppm; Antiblock: No; Slip: No

Information provided by Sahara International Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Vinyl Acetate Content 18 %ASTM D5594
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 610 %ASTM D882
Film Elongation at Break, TD 630 %ASTM D882
Film Tensile Strength at Break, MD 20.0 MPaASTM D882
Film Tensile Strength at Break, TD 27.0 MPaASTM D882
1% Secant Modulus, MD 48.0 MPaASTM D882
1% Secant Modulus, TD 50.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 85.0 °CASTM D3418
Vicat Softening Point 64.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.8 %ASTM D1003
Gloss 120 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPCH008 / 285321

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.