MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-LOY™ Compound W3000XXJ Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP STAT-LOY W3000XXJ compound is based on Polybutylene Terephthalate (PBT) resin containing proprietary fillers. Added features of this grade include: Permanently Anti-Static, Colorable, Healthcare, Low Extractables.

Features: Low Extractable,Healthcare,Colorable,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Density 1.27 g/ccASTM D792
Moisture Absorption 0.0500 %Injection Molding
 0.230 %23°C/50% RH/24 hrs; ASTM D570
 0.370 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 41.0 MPa5 mm/min; ASTM D638
 42.0 MPa5 mm/min; ISO 527
Elongation at Break 4.3 %5 mm/min; ASTM D638
 9.6 %5 mm/min; ISO 527
Elongation at Yield 8.5 %5 mm/min; ISO 527
Tensile Modulus 1880 MPa1 mm/min; ISO 527
 1930 MPa50 mm/min; ASTM D638
Flexural Strength 61.0 MPaISO 178
Flexural Modulus 1890 MPa2 mm/min; ISO 178
 1940 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 61.0 JASTM D256
Izod Impact, Unnotched 1400 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 89.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+11 - 1.00e+13 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 115 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 128 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 139 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 157 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 55.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 215 - 225 °C
Zone 3 220 - 230 °C
Melt Temperature 220 - 230 °CInjection Molding
Mold Temperature 10.0 - 50.0 °C
Drying Temperature 110 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81429 / 289376

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.