MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem RUBAMIN ZINC BORATE Flame Retardant
Categories: Other Engineering Material

Material Notes: Product Description: Zinc Borate is an important additive to help achieve excellent flame resistance in rubber articles. It is a free-flowing powder that disperses easily. Zinc Borate can be added to any flame retardant system and will improve flame test results with minimal effect on compound properties. Zinc borate will form a glassy char at high temperatures that prevents flame propagation. It also releases water of hydration similar to ATH. Zinc borate is a synergist with antimony oxide and halogenated flame-retardants as well as ATH. The combined ingredients will have better flame resistance than the separate materials would have. Zinc borate helps in compounding halogen-free, flame-resistant rubber that generates minimum acidic smoke.

Applications: Zinc borate works in concert with virtually all other flame retarders. The synergy with antimony oxide allows ½ as much antimony oxide to be used and obtain comparable results. As it becomes more apparent that smoke kills as many people as an actual fire, low-smoke flame retardance is becoming critical. Zinc borate is an important part of low-smoke formulas. 5-10 phr is a recommended starting point. Other parts of a low smoke formula include ATH and/or magnesium hydroxide as water-donating fillers and a phosphorus source to aid char formation. Akrochem offers all of these fire retardant ingredients. Zinc borate is also a potent anti-fungal and anti-bacterial additive. 2% zinc borate in a compound can provide a distinct decrease in mold growth.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.77 g/cc
 
Descriptive Properties
Appearancefree-flowing white powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH259 / 315177

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.