MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
RAMPF RAKU® TOOL InnoClear™ OC-5284 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Water-clear, semi-rigid polyurethane formulated

Key Properties:

  • Excellent physical properties
  • Free of mercury, MOCA or TDI
  • Excellent optical clarity as well as U.V. stability
Applications:
  • For room temperature hand-batch or vacuum assisted casting methods
Cure 1: 24 hours at 77°F
Cure 2: 7 days at 77°F + 8 hour at 175°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccHardener; ASTM D-792
 1.08 g/ccCure 2; ASTM D-792
 1.10 g/ccCure 1; ASTM D-792
 1.16 g/ccResin; ASTM D-792
Viscosity 900 cPResin; ASTM D-2393
 1200 cPMix; ASTM D-2393
 3300 cPHardener; ASTM D-2393
Linear Mold Shrinkage 0.0010 - 0.0020 in/inCure 1; ASTM D-2566
 0.0010 - 0.0020 in/inCure 2; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 90Cure 1; ASTM D-2240
 80 - 90Cure 2; ASTM D-2240
Tensile Strength 10100 psiCure 1; ASTM D-638
 11000 psiCure 2; ASTM D-638
Elongation at Break 8.0 %Cure 1; ASTM D-638
 10 %Cure 2; ASTM D-638
Flexural Strength 9000 psiCure 1; ASTM D-790
 13500 psiCure 2; ASTM D-790
Flexural Modulus 275000 psiCure 1; ASTM D-790
 275000 psiCure 2; ASTM D-790
Izod Impact, Notched 0.900 ft-lb/inCure 2; ASTM D-256
 1.10 ft-lb/inCure 1; ASTM D-256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 54.0 °CCure 1; ASTM D-648
 89.0 °CCure 2; ASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 - 24.0 hourMix, Demold time
Gel Time 40.0 - 60.0 minMix
 
Descriptive Properties
AspectWater ClearCure 1
 Water ClearCure 2
Mix Ratio100:50Resin: Hardener, Weight
 100:55Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAMPF131 / 317731

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.