SABIC® PP QR675K is a highly transparent random copolymer with good antistatic properties
with excellent flow behaviour. This grade combines improved aesthetics of the finished articles with low
temperature processability. Part aesthetics are not affected by the lower processing temperatures, providing for a
broader operating window. The SABIC® PP QR675K results in excellent demoulding characteristics and has
a good stiffness to impact ratio.
Application: SABIC® PP QR675K is mainly used in injection moulding processes. The SABIC® PP QR675K
aims at transparent applications were higher MFI’s with good flow are required. Its intended applications
include injection moulded housewares, office & home storage boxes, thin wall packaging and media
packaging.
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/
medical applications.
This grade material is UL registered under File E111275 / IMDS 80775790Information provided by SABIC |