Tefzel™ ETFE film is a transparent, thermoplastic film that can be heat sealed, thermoformed, vacuum formed, heat bonded, welded, metalized, laminated (combined with dozens of other materials), and used as an excellent hot melt adhesive. This wide variety of fabrication possibilities combines with the following important properties to offer a unique balance of capabilities not available in other plastic films. Features: Chemical Compatibility, Electrical Reliability, Wide Thermal Range, Mechanical Toughness, Long Time Weather ability, Reliability.Information provided by Chemours. |