MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Rynite® GW525CS1 WT709 PET-GF25 FR(16)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: 25% Glass Reinforced, Flame Retardant, Polyethylene Terephthalate with Improved Glow Wire Performance

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.67 g/ccISO 1183
Viscosity 210000 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
Melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPaISO 527-1/-2
Elongation at Break 2.0 %ISO 527-1/-2
Tensile Modulus 11000 MPaISO 527-1/-2
Poissons Ratio 0.34
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 250 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 230 °CISO 75-1/-2
Flammability, UL94 V-2
@Thickness 0.800 mm
IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °COptimum, Injection
 270 - 290 °CRange, Injection
Mold Temperature 120 - 140 °CInjection
 140 °COptimum, Injection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %Injection
Hold Pressure >= 80.0 MPaInjection
 
Descriptive Properties
AdditivesFlame retardant
 Release agent
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
PolymerPET-GF25 FR(16)
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
 Europe
 Near East/Africa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4849a / 291005

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.