Flame retardant PC alloy grade. Filler reinforced, High Stiffness, Dimensional Precision. Polycarbonate is known for its high impact resistance, good transparency and heat resistance, and superb precision and electrical properties. TARFLON is used in a wide range of applications such as house wares, office equipment , mobile devices, communications equipment, display devices such as LCD backlight parts, automotive, lighting and many fields. Information provided by Idemitsu Losan Co. |