Daplen™ EH119AEB is a 12% mineral filled elastomer modified polypropylene compound intended for injection molding. Applications: Daplen EH119AEB has been developed especially for the car industry to be used in automotive exterior parts. - Automotive exterior applications
- Bumpers
- Exterior trims
Special Features: - High impact strength at low temperature
- Suitable for applications, which require low expansion over a broad temperature scale
- Excellent flowability
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time.Information provided by Borealis AG |