NOCOLOK® Precoating can be used in mixture with NOCOLOK® Flux or NOCOLOK® Zn Flux and water to improve adhesion of the flux coating. Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appliances Information provided by Solvay |