System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ LUBRICOMP™ Compound CG002XXN Polystyrene (PS)
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
Material Notes:
LNP LUBRICOMP CG002XXN compound is based on Polystyrene (PS) resin containing graphite. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.10
g/cc
1.10
g/cc
ASTM D792
Density
1.10
g/cc
0.0397
lb/in³
ISO 1183
Water Absorption
0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ASTM D570
Moisture Absorption
0.0200 %
0.0200 %
Injection Molding
0.0400 %
0.0400 %
23°C/50% RH/24 hrs; ASTM D570
0.0300 - 0.0500 %
0.0300 - 0.0500 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
0.030 - 0.050 %
0.030 - 0.050 %
ISO 62-1
Viscosity
21
cP
@Load 5.00 kg,
Temperature 230 °C
21
cP
@Load 11.0 lb,
Temperature 446 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
SABIC method
Linear Mold Shrinkage, Transverse
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
SABIC method
Melt Flow
20
g/10 min
@Load 5.00 kg,
Temperature 230 °C
20
g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
45.0
MPa
6530
psi
5 mm/min; ISO 527
47.0
MPa
6820
psi
5 mm/min; ASTM D638
Elongation at Break
2.0 %
2.0 %
5 mm/min; ASTM D638
2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus
4.10
GPa
595
ksi
1 mm/min; ISO 527
4.20
GPa
609
ksi
5 mm/min; ASTM D638
Flexural Strength
72.0
MPa
10400
psi
break, 2mm/min; ISO 178
74.0
MPa
10700
psi
brk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
4.00
GPa
580
ksi
1.3 mm/min, 50 mm span; ASTM D790
4.00
GPa
580
ksi
2 mm/min; ISO 178
Izod Impact Notched
13.0
J
9.59
ft-lb
ASTM D256
Izod Impact, Unnotched
1.11
J/cm
2.08
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
2.00
kJ/m²
0.952
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
8.00
kJ/m²
3.81
ft-lb/in²
80*10*4; ISO 180/1U
Charpy Impact Unnotched
0.900
J/cm²
4.28
ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
0.100
J/cm²
0.476
ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
67.6
µm/m-°C
@Temperature 23.0 - 60.0 °C
37.6
µin/in-°F
@Temperature 73.4 - 140 °F
ASTM E831
67.6
µm/m-°C
@Temperature 23.0 - 60.0 °C
37.6
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow
78.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
43.3
µin/in-°F
@Temperature 73.4 - 140 °F
ASTM E831
78.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
43.3
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
95.0
°C
203
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
95.0
°C
@Thickness 3.20 mm
203
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
85.0
°C
185
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
85.0
°C
@Thickness 3.20 mm
185
°F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point
99.0
°C
210
°F
Rate B/50; ASTM D1525
99.0
°C
210
°F
Rate B/50; ISO 306
100
°C
212
°F
Rate B/120; ISO 306
Processing Properties
Metric
English
Comments
Nozzle Temperature
235
-
265
°C
455
-
509
°F
Zone 2
230
-
250
°C
446
-
482
°F
Zone 3
240
-
270
°C
464
-
518
°F
Melt Temperature
240
-
270
°C
464
-
518
°F
Injection Molding
Mold Temperature
40.0
-
60.0
°C
104
-
140
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
-
6.00
hour
4.00
-
6.00
hour
Injection Molding
48.0
hour
48.0
hour
Cumulative; Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Precipitation Temperature
40.0
-
60.0
°C
104
-
140
°F
Hopper Temperature
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH80670 / 288617
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.