Product Description: Self Extinguishing Grade. Characteristics: High flow, Flame Retardant Cl, Br, Sb Free. Availability: Asia Pacific; Europe; North America Additive: Flame Retardant Features: Antimony Free; Bromine Free; Chlorine Free; Flame Retardant; High Flow; Self Extinguishing Agency Rating: EC 1907/2006 (REACH) RoHS Compliance: RoHS Compliant UL File Number: E162823Information provided by Formosa Chemicals & Fiber Corporation |