MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PTFE N100
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: The main industry for the use of PTFE N100 is food and beverage. The primary objective in the food production and packaging industry is to deliver high quality, healthy and safe products. This highly regulated market requires compliance with international standards and can quickly become a major threat to the company if these standards are not met. Product recalls can and have led to worst-case scenarios for producers. Angst + Pfister offers high-quality engineering plastic components which meet these requirements, such as sliding elements and guides etc., sealing elements such as flat seals and wipers etc., electrical insulating parts in the high-frequency or high-voltage range as well as non-stick coating in food and filling plants. Recommended material is PTFE N100. The use of PTFE N100 is particu¬larly suitable for these conditions, especially since it is equipped with the necessary certifications, has excellent resistance to very high and very low temperatures, has an extremely low coefficient of sliding friction, an anti-adhesive surface, is exceptionally resistant to chemicals, shows very good dielectric behaviour and is weatherproof.

Benefits:

  • Listed und approved by NSF/ANSI 61, Drinking Water System Components – Health Effects.
  • Additionally, compliance with common Eurpean drinking water approvals
  • Certified for Sealing Materials in cold water with a testing tem¬perature of up to +23°C and commercial hot water with a testing temperature of up to +82°C.
  • Extremely low coefficient of sliding friction and anti-adhesive surface
  • Exceptionally resistant to chemicals
  • Traceable

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.18 g/cc
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
 280 °Cshort-term
Minimum Service Temperature, Air -200 °C
 
Descriptive Properties
Colornatural (white)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP112 / 250610

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.