MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin LTA6020 Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ LTA6020 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm, 5VB at 2mm, and V0 at 1.5mm. NORYL LTA6020 exhibits good dimensional stability over a wide temperature range, high heat performance, low moisture uptake, and offers long-term aging / retention of mechanical properties. It is an excellent candidate for solar / photovoltaic (PV) junction boxes and outdoor electrical enclosures.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Density 1.13 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
 20 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 57.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 71.0 MPa50 mm/min; ISO 527
 72.0 MPa50 mm/min; ASTM D638
Elongation at Break 8.0 %50 mm/min; ISO 527
Elongation at Yield 4.0 %50 mm/min; ISO 527
 6.0 %50 mm/min; ASTM D638
Tensile Modulus 2680 MPa1 mm/min; ISO 527
Flexural Strength 105 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
 105 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2580 MPa2.6 mm/min, 100 mm span; ASTM D790
 2600 MPa2 mm/min; ISO 178
Izod Impact Notched 220 JASTM D256
Izod Impact, Notched (ISO) 16.0 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -20.0 °C
80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -10.0 °C
80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Charpy Impact Unnotched 18.0 kJ/m²ISO 179/2C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.00 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=1.00 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 123 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 126 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 144 °CRate B/120; ISO 306
 155 °CRate A/120; ISO 306
UL RTI, Electrical 125 °CUL 746B
UL RTI, Mechanical with Impact 125 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 V-1
@Thickness >=1.00 mm
UL 94
 V-0
@Thickness >=1.50 mm
UL 94
 5VB
@Thickness >=2.00 mm
UL 94
 5VA
@Thickness >=2.50 mm
UL 94
Glow Wire Ignition Temperature 825 °C
@Thickness 1.00 mm
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Zone 2 280 - 300 °C
Zone 3 270 - 290 °C
Melt Temperature 280 - 300 °CInjection Molding
Mold Temperature 80.0 - 100 °C
Drying Temperature 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82348 / 290295

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.