MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX973 Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 973 resin is a conductive, non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized to allow for in- or on-line primer-less electrostatic and powder coat painting. NORYL GTX973 resin exhibits high impact resistance and strength and is an excellent candidate for automotive painted applications such as body panels, fenders, and tank flaps.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Low Warpage,Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Density 1.09 g/ccISO 1183
Water Absorption 0.81 %
@Time 86400 sec
ASTM D570
 0.81 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0700 %Injection Molding
 0.210 %23°C/50% RH/24 hrs; ISO 62-4
Moisture Absorption at Equilibrium 0.61 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation 2.24 %ASTM D570
 2.24 %ISO 62-1
Viscosity 4.7 cP
@Load 2.16 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
 12 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.016 cm/cm24hrs; ASTM D955
 0.016 cm/cm24hrs; ISO 294
 0.014 - 0.017 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0169 cm/cm24hrs; ASTM D955
 0.0169 cm/cm24hrs; ISO 294
 0.012 - 0.015 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 280 °C
ASTM D1238
 20 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPa50 mm/min; ASTM D638
 56.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 61.0 MPa50 mm/min; ASTM D638
 64.0 MPa50 mm/min; ISO 527
Elongation at Break 37 %50 mm/min; ASTM D638
 41 %50 mm/min; ISO 527
Elongation at Yield 4.8 %50 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2300 MPa50 mm/min; ASTM D638
 2300 MPa1 mm/min; ISO 527
Flexural Strength 99.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2230 MPa1.3 mm/min, 50 mm span; ASTM D790
 2380 MPa2 mm/min; ISO 178
Izod Impact Notched 138 JASTM D256
 80.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 - 10000 ohm-cmSABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 92.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ASTM E831
 92.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 95.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ASTM E831
 95.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 190 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 198 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 136 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 199 °CRate B/50; ASTM D1525
 200 °CRate B/50; ISO 306
 245 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 310 °C
Zone 2 280 - 300 °C
Zone 3 290 - 320 °C
Melt Temperature 290 - 320 °CInjection Molding
Mold Temperature 100 - 120 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82187 / 290134

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.